Steel, Corrosion Resistant, Bars and Wire 18Cr – 9.0Ni (302) Solution Heat Treated, Cold Drawn and Stress Relieved 125 ksi (862 MPa) Tensile Strength
standard by SAE International, 07/27/2018
SAE AMS5637J – Steel, Corrosion Resistant, Bars and Wire 18Cr – 9.0Ni (302) Solution Heat Treated, Cold Drawn and Stress Relieved 125 ksi (862 MPa) Tensile Strength
This specification covers a corrosion resistant steel in the form of bars and wire 0.75 inch (19 mm) and under in nominal diameter or distance between parallel sides (see 8.4).